Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.427 J/cm @Temperature 23.0 °C |
0.800 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.800 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® PS-1000 Polybutylene Terephthalate (PBT)
(discontinued **) Description/Features:UL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Enviramid™ N1320HL BK Post Consumer Recycle Nylon 66, 20% Glass Filled Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CH020-03 Polypropylene, Homopolymer, BOPP COPYLENE™ CH020-03 is a polypropylene homopolymer resin designed for BOPP (biaxially oriented polypropylene) film extrusion applicationsApplications: Bags & Pouches, Raffia/Tapes/Strapping, Peelabl.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
Global CPP-130 30% CaC03 Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 0.427 J/cm @Diameter 0.125 mm, Temperature -20.0 °C |
0.800 ft-lb/in @Diameter 0.00492 in, Temperature -4.00 °F |
bar; ASTM D256 |
Ineos L12Z-01 Polypropylene Impact Copolymer Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provi.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-130 Polypropylene Homopolymer, 30% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF/B40 L 40% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 40% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: Natural ColorInformation provided by TP.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 CM30 L 30% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.427 J/cm | 0.800 ft-lb/in | ASTM D256 |
Washington Penn Medium Impact Copolymer 50% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.800 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® AT-25GF-10MN/000 NATURAL Acetal-Copolymer, Glass/Mineral Filled
(discontinued **) Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |