Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.422 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.790 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HI2100M PBT+GF10% Description: Injection Molding, PBT+GF10%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 65997-17-3, 155123-66-3 and 30965-26-5Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.422 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 0.790 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
Izod Impact, Notched | 0.422 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.790 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Sumitomo Chemical Sumipex® BF3 Acrylic Resin, GP Blow Molding Grade Product CharacteristicsExcellent WeatherabilityHigh TransparencyGood Heat ResistanceInformation provided by Calsak Corporation |
|||
Izod Impact, Notched | 0.422 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.790 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Sumitomo Chemical Sumipex® LG Acrylic Resin, High Flow Product CharacteristicsHigh FlowInformation provided by Calsak Corporation |
|||
Izod Impact, Notched | 0.422 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.790 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow Product CharacteristicsHigh FlowInformation provided by Calsak Corporation |
|||
Izod Impact, Notched | 0.422 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.790 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Sumitomo Chemical Sumipex® MH Acrylic Resin, Heat Resistant Product CharacteristicsExtrusion GradeHeat ResistantInformation provided by Calsak Corporation |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Cheng Yu Plastic PP226 Flame Retardant Polypropylene, Medium Impact |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer HP0334W20L Wollastonite Reinforced |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334M40L Mica Reinforced |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336G20CL Glass Reinforced Coupled |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M20L Mica Reinforced |
|||
Izod Impact, Notched | 0.422 J/cm | 0.790 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® K365GM 60% Glass Fiber/Calcium Carbonate Reinforced General Purpose PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |