Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.410 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.768 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
Proto3000 Duraform® GF Selective Laser Sintering (SLS®) Prototyping Polymer Description: Glass-filled polyamide (nylon) material for real-world physical testing and functional useFeatures:Excellent mechanical stiffnessElevated temperature resistanceDimensionally stableEasy-.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
North Wood Plastics PS with 20% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Notched | 0.410 J/cm @Thickness 3.17 mm |
0.768 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
(discontinued **) Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding. Molded parts provide excellent part detail on fast production cycles. Molded parts have excellent c.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36L PA 66 LNP* LUBRICOMP* RBL36L is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features s of this grade are: Low Extractable, Wear Resistant. |
|||
Izod Impact, Notched | 0.410 J/cm @Temperature 23.0 °C |
0.768 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This .. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 0.410 J/cm @Temperature 23.0 °C |
0.768 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp JF003L PES LNP* Thermocomp* JF003L is a compound based on Polyethersulfone (PES) containing Glass Fiber. Characteristics of this grade are Low Extractable.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Notched | 0.410 J/cm @Temperature 23.0 °C |
0.768 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled productThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
Plenco 6990 Phenolic, Briquette, Compression Molded PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |
|||
Izod Impact, Notched | 0.410 J/cm @Thickness 3.17 mm |
0.768 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chevron Phillips K-Resin® KR03 Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give excellent part detail on fast production cycles. It can be t.. |
|||
Izod Impact, Notched | 0.410 J/cm @Thickness 3.17 mm |
0.768 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR03 to facilitate printing.Customer Benefits: This SBC is easily processed by injection molding or sheet extrusion and molded parts give .. |
|||
Izod Impact, Notched | 0.410 J/cm @Thickness 3.17 mm |
0.768 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chevron Phillips K-Resin® KR05 Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene CopolymerCustomer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good s.. |
|||
Izod Impact, Notched | 0.410 J/cm @Thickness 3.17 mm |
0.768 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing.Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Fin.. |
|||
Izod Impact, Notched | 0.410 J/cm @Temperature 23.0 °C |
0.768 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
3D Systems DuraForm® GF Glass Filled Nylon For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM-D256 |
Braskem H 611 HOMO Polypropylene Homopolymer H 611 is a low melt flow rate homopolymer that was specially designed for exposure to solar light. This product exhibits good processability and high melt resistance. It is designed for raffia extru.. |
|||
Izod Impact, Notched | 0.410 J/cm @Temperature -30.0 °C |
0.768 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.410 J/cm | 0.768 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |