Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Izod Impact, Notched | 0.392 - 4.00 J/cm | 0.735 - 7.49 ft-lb/in | Average value: 1.77 J/cm Grade Count:104 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Izod Impact, Notched | 0.392 - 100 J/cm | 0.735 - 187 ft-lb/in | Average value: 7.09 J/cm Grade Count:113 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Shinil Chemical SHINSTAT PMMA Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Shinil Chemical SHINSTRA PC/PET TES Structural Polymer Car Spoiler SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.35 mm |
0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.35 mm |
0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210P Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210P is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL G175D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH40FR2 Flame Retardant Heat Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Asia Technology Pioneers CAP 101 PP Nanocomposite Description: CAP101 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 3010FW Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm |
0.735 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211D Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 23.0 °C |
0.735 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H ME9180 HDPE Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS N.. |
|||
Izod Impact, Notched | 0.392 J/cm @Temperature 23.0 °C |
0.735 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |