Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
Ovation Polymers UTTAP QU BM513 GF BM Nylon, 13% Glass Reinforced Glass reinforced (13 %) High Temperature Polyamide - Blow Molding grade with excellent chemical resistance, improved flow and high HDT. *All properties are measured after 48 hours of conditioning at.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.18 mm |
0.701 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.18 mm |
0.701 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.18 mm |
0.701 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Notched | 0.374 - 0.374 J/cm @Temperature -30.0 - -30.0 °C |
0.701 - 0.701 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 2.37 J/cm Grade Count:1 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.374 - 0.374 J/cm @Thickness 3.17 - 3.17 mm |
0.701 - 0.701 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 2.37 J/cm Grade Count:1 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5872 Polyetherimide, 25% PTFE Lubricant
(discontinued **) Not stand-alone resin: Compounding/ concentrate for wear resistance. Will be commercialized as UF2500.Features: Lubricated, Good Wear ResistanceForms: PelletsInformation provided by LNP, a GE Plasti.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256A |
Total PPH 3230 Polypropylene, Blow Molding Grade Homopolymer blow molding gradeLubricated - Fina 3230 offers superior core rod release, eliminating the need for additional lubricant.High Purity - Fina 3230 features minimum taste and odor and optim.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256A |
Total PPR 3230XZ Polypropylene, Blow Molding Grade Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256A |
Dow NRD6-589 Polypropylene Random Copolymer Resin DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256A |
Braskem INSPIRE™ 404 Performance Polypropylene Polymer INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of .. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan.. |
|||
Izod Impact, Notched | 0.374 J/cm @Thickness 3.18 mm |
0.701 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discontinu Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |