Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.670 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.358 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.670 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Therma-Tech™ PI-5000 TC Polyetherimide (PEI)  (discontinued **)
Description/Features:Thermally ConductiveElectrically ConductiveUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved