Izod Impact, Notched |
0.352 J/cm @Thickness 3.17 mm
|
0.660 ft-lb/in @Thickness 0.125 in
|
ASTM D256 |
Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial
Information provided by FIBERFIL Engineered Plastics |
Izod Impact, Notched |
0.352 J/cm @Temperature 22.8 °C
|
0.660 ft-lb/in @Temperature 73.0 °F
|
ASTM D256 |
Teknor Apex Sinpolene GPP1610 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 10% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334T20L1 Talc Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336T10L Talc Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W20L Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W30L Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336W40L1 Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339C10L Calcium Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339C20L Calcium Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339C30L Calcium Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339C40L Calcium Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339G5M25CL Glass/Mineral Reinforced Coupled
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339W10L1 Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Copolymer HP0335W40L Wollastonite Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339M10L Mica Reinforced
|
Izod Impact, Notched |
0.352 J/cm |
0.660 ft-lb/in |
ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0339M20L Mica Reinforced
|