Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.350 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.656 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Novablend™ 5035 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC PP 521P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 521P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm | 0.656 - 0.843 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc.. |
|||
Izod Impact, Notched | 0.350 - 0.800 J/cm @Temperature -40.0 - 0.000 °C |
0.656 - 1.50 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.531 J/cm Grade Count:6 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.350 - 1.60 J/cm | 0.656 - 3.00 ft-lb/in | Average value: 0.780 J/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Notched | 0.350 - 981 J/cm | 0.656 - 1840 ft-lb/in | Average value: 7.00 J/cm Grade Count:191 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.350 - 0.350 J/cm @Temperature -40.0 - -20.0 °C |
0.656 - 0.656 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.350 J/cm Grade Count:1 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HV-1010 General Purpose PBT, Unreinforced, High Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 1310 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ZM3640 PPE+PS (Asia Pacific) |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Styrolution Styrolux® 693 D SBC Description: Styrolux® 693 D is a clear styrene-butadiene copolymer (SBC) with a well balanced combination of toughness and clarity. Styrolux® 693 D is mainly used for thermoformed articles, e.. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -30.0 °C |
0.656 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East) 10% GF FR PBT/PC Blend |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Asia Pacific) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature -40.0 °C |
0.656 ft-lb/in @Temperature -40.0 °F |
ISO 180 Method A |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.350 J/cm @Temperature 23.0 °C |
0.656 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter PF340S6 PBT, 30% Glass Beads 30% Glass beads reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM-D256 |
Braskem H 503HS HOMO Polypropylene Homopolymer H 503HS is a low melt flow rate homopolymer for general purpose. It is designed for raffia extrusion and fiber extrusion. This product exhibits excellent processability, high speed production with g.. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM-D256 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Izod Impact, Notched | 0.350 - 0.450 J/cm @Temperature -40.0 - -40.0 °C |
0.656 - 0.843 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.400 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched | 0.350 - 1.08 J/cm | 0.656 - 2.02 ft-lb/in | Average value: 0.713 J/cm Grade Count:32 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.350 J/cm | 0.656 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |