Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |