Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 2008 X Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.20 mm, Temperature 22.8 °C |
0.600 ft-lb/in @Thickness 0.126 in, Temperature 73.0 °F |
injection molded ASTM Type 1 specimen; ASTM D256 |
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 22.8 °C |
0.600 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Sintimid™ V Unfilled Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Izod Impact, Notched | 0.320 - 1.12 J/cm | 0.600 - 2.10 ft-lb/in | Average value: 0.767 J/cm Grade Count:8 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched | 0.320 - 2.40 J/cm | 0.600 - 4.50 ft-lb/in | Average value: 0.882 J/cm Grade Count:64 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE 0226 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PS 06001 Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler/Unspecified FillerReinfor.Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6 SF76 L Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite (76%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Washington Penn High Modulus Polypropylene Homopolymer 40% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Washington Penn Homopolymer Polypropylene 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Diamond Polymers ASA TWP 155 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 0.000 °C |
0.600 ft-lb/in @Temperature 32.0 °F |
molded and tested in accordance with ASTM D 4101; ASTM D256A |
Dow H110-02N Polypropylene Resin DOW H110-02N is intended for use in extrusion and thermoforming processes. It is especially suited for applications where improved melt strength and clarity are desired.Information provided by DowD.. |
|||
Izod Impact, Notched | >= 0.320 J/cm | >= 0.600 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPPC 2008 C BLK Polypropylene, Calcium Filled Product Information: Calcium Carbonate Filled PP Grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. Our BP RPP C series product line ranges fro.. |
|||
Izod Impact, Notched | 0.320 - 0.481 J/cm | 0.600 - 0.900 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.600 ft-lb/in | ASTM D256 |
Asahi Kasei Thermofil N-40MF-1600 40% Mineral Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm |
0.600 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR HS Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized, Halogen Free and LubricatedTPCI# 9857101Information provided by TP Composi.. |