Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.294 J/cm @Temperature 23.0 °C |
0.550 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers OpteSTAT™ NC PPS 7010 Polyphenylenesulfide based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | |
XX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 22.8 °C |
0.550 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5130 Talc Filled Homopolymer Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech |
|||
Izod Impact, Notched | 0.294 J/cm @Temperature 22.8 °C |
0.550 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP5321 Mica Reinforced Homopolymer Information provided by Spartech |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SRP 8602 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Conduit; Piping; Profiles Forms: Granules Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.550 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Izod Impact, Notched | 0.294 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.550 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
ExxonMobil PP1105E1 Homopolymer Product Description: High melt flow rate homopolymer. Particularly suitable for general purpose injection molding.Availability: North America Features:Controlled RheologyGeneral PurposeGood Proces.. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFPP 2010 Calcium Carbonate Filled Polypropylene AAROPRENE® CFPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.294 J/cm | 0.550 ft-lb/in | |
Abatron AboCast/AboCure 8006-11 Epoxy AboCast/AboCure 8006-11 is a clear dielectric casting, adhesive, and encapsulating compound. It is a 2-component, radiation-resistant, low-viscosity plasticized epoxy system. It is virtually unaffec.. |
|||
Izod Impact, Notched | >= 0.294 J/cm | >= 0.550 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 2122UV-M-31 is a black 40% talc filled polypropylene. It is weather and urethane contact resistant and contains a mold release. Information provided by A. Schulman. |