Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.290 J/cm @Temperature -40.0 °C |
0.543 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar Copolyester K3000 PETG Copolyester
(discontinued **) EASTAR K3000 Copolyester is a cost effective, high-performance, water-clear material that provides the necessary performance for the appliance standards. Other desirable characteristics are good ch.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plenco 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **) Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou.. |
|||
Izod Impact, Notched | 0.290 - 6.03 J/cm | 0.543 - 11.3 ft-lb/in | Average value: 1.10 J/cm Grade Count:126 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Notched | 0.290 - 0.850 J/cm | 0.543 - 1.59 ft-lb/in | Average value: 0.647 J/cm Grade Count:3 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TF302 Wear Modified Acetal Resin PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TF304 Wear Modified Acetal Resin PTFE powder added, improved wear property. Applications: High speed, high load and wear resistant products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL ZWM2411 PPE+PS (Asia Pacific) Modified PPO*, 30% mineral filled product, V-1@1.5mm, HDT 125degC, low warpage product, BK color only |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
UBE P7115U Electronic Grade Nylon Copolymer Powder Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
UBE 7115U Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.290 J/cm @Thickness 3.17 mm |
0.543 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM-D256 |
Braskem PH 0242 HOMO Polypropylene Homopolymer PH 0242 is a low melt flow rate homopolymer produced by compression molding. This resin exhibits excellent processability and excellent stiffness/impact strength balance. Its applications include co.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T355J Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T357 Electrical Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced A flame retardant PBT polyester with 45% glass reinforcement, mineral filled.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.290 - 0.961 J/cm | 0.543 - 1.80 ft-lb/in | Average value: 0.565 J/cm Grade Count:80 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM-D256 |
Braskem H 203 HOMO Polypropylene Homopolymer H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T385J General Purpose Phenolic Molding Compound ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at.. |
|||
Izod Impact, Notched | 0.290 J/cm | 0.543 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America. |