Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.250 - 6.41 J/cm | 0.468 - 12.0 ft-lb/in | Average value: 1.05 J/cm Grade Count:69 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D256A |
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **) Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Ineos Nova Zylar® 330 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:Clarity and stiffness Good heat distortion resistance Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class .. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 23.0 °C |
0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H250FG Polypropylene REPOL Polypropylene H250FG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester Akestra™ is a thermoplastic with a sparkling glass-like appearance. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “di.. |
|||
Izod Impact, Notched | 0.250 J/cm - NB | 0.468 ft-lb/in - NB | Average value: 2.26 J/cm Grade Count:17 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.468 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.275 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Plaslok 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 301 is a two-stage, woodflour and flo.. |
|||
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | ASTM D256 |
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness... |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 23.0 °C |
0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 301 Injection Molding Polypropylene Description: H 301 is a high melt flow rate homopolymer designed for injection moulding and fiber extrusion. This product exhibits excellent processability with good melt strength and stiffness/impa.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature >=23.0 °C |
0.468 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® T 12 EV Polypropylene Homopolymer CAPILENE® T 12 EV is a polypropylene homopolymer with narrow molecular weight distribution, controlled rheology, intended for fiber applications. It is characterized by easy processing, very good m.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Carmel Olefins CAPILENE® T 89 E Polypropylene Homopolymer Description: CAPILENE® T 89 E is a high melt flow rate homopolymer for continuous filaments, staple fibers and for injection molding. It is formulated with an anti-gasfading stabilization package.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature >=23.0 °C |
0.468 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® U 77 AV Polypropylene Homopolymer CAPILENE® U 77 AV is a high melt flow rate polypropylene homopolymer controlled rheology, designed for injection molding of products with long flow length. It is specially formulated with antistati.. |
|||
Izod Impact, Notched | >= 0.250 J/cm | >= 0.468 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester Excellent appearance, clarity, hydrolytic stability, heat resistance and high strength. Used for extrusion and injection molded articles, blow molding, films and sheets. It can be used as a polyst.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 23.0 °C |
0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 306 Injection Molding Polypropylene Description: H 306 is a medium melt flow rate additivated homopolymer used for general purposes. It suitable for injection moulding and fiber extrusion. This product exhibits excellent processabilit.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu.. |
|||
Izod Impact, Notched | 0.250 - 0.340 J/cm @Thickness 6.35 mm |
0.468 - 0.637 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.250 - 1.35 J/cm @Diameter 0.125 - 3.17 mm |
0.468 - 2.53 ft-lb/in @Diameter 0.00492 - 0.125 in |
Average value: 0.794 J/cm Grade Count:11 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.250 - 6.00 J/cm | 0.468 - 11.2 ft-lb/in | Average value: 0.723 J/cm Grade Count:95 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |