Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC PP 510P Polypropylene Homopolymer for Fiber Applications Product Description: PP 510P is a homopolymer specially designed for fiber extrusion applications with the following features:Consistent processabilityGood thread line stabilityGood color consisten.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC PP 511A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 511A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 511A has the following features:Consis.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -30.0 °C |
0.412 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | 0.220 - 0.350 J/cm | 0.412 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | >= 0.220 J/cm @Temperature 23.0 °C |
>= 0.412 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 2060V (60118) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Izod Impact, Notched | 0.220 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.412 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ ST9620-0020 ES Red Liquid Crystal Polymer + PPS (LCP+PPS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature 23.0 °C |
0.412 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol H350FG Polypropylene REPOL Polypropylene H350FG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Ineos H03W-01 Polypropylene, Gas Phase Polymerized H03W-01 (formerly Fortilene® HG3253) belongs to the new generation of polypropylenes produced by gas phase polymerization. This nominal 4 melt flow index product is specifically designed for fib.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -40.0 °C |
0.412 ft-lb/in @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CA187 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balanceApplications:.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ EP 5001C(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America SI 9002N-1 Silicone Compound Short fibergass reinforced silicone molding compound which offers moderate strength properties, dimensional stability, and excellent long-term thermal stability at elevated temperatures.Information .. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Plenco 1510 Polyester, Pellet, Injection Molded PLENCO 01510 is a mineral filled, pelletized polyester molding compound, which offers an excellent combination of electrical properties and dimensional stability. UL recognized under component file .. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1068-32 Black40% Mineral Filled Polypropylene DescriptionPolyfort® FPP 1068-32 Black is a 40% mineral filled polypropylene designed for use when improved heat resistance, dimensional stability and high stiffness is needed. ApplicationApplicati.. |
|||
Izod Impact, Notched | 0.220 - 0.260 J/cm | 0.412 - 0.487 ft-lb/in | ASTM D256A |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3 Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Izod Impact, Notched | 0.220 - 0.390 J/cm | 0.412 - 0.731 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Izod Impact, Notched | 0.220 J/cm @Thickness 3.20 mm |
0.412 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® GL2200 ABS Good Flow Grade High impact, Easy processingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.220 - 0.400 J/cm | 0.412 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Izod Impact, Notched | 0.220 J/cm @Diameter 3.17 mm |
0.412 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Accpro® 9934 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, Antistatic, High surface hardness, Stain resistanceComplies with FDA specification, Title 21, CFR 177.1520.Typica.. |
|||
Izod Impact, Notched | 0.220 J/cm | 0.412 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |
|||
Izod Impact, Notched | 0.220 - 0.801 J/cm | 0.412 - 1.50 ft-lb/in | Average value: 0.471 J/cm Grade Count:18 |
Overview of materials for Polypropylene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched | 0.220 - 12.0 J/cm | 0.412 - 22.5 ft-lb/in | Average value: 0.998 J/cm Grade Count:29 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |