Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.215 J/cm | 0.403 ft-lb/in | ASTM D256 |
Flint Hills 21N2A Homopolymer Polypropylene Features: FDA Compliant, High Flexural Modulus and High Heat Deflection TemperatureApplications: Thermoforming, Extrusion, Blow MoldingInformation provided by Flint Hills Resources. |
|||
Izod Impact, Notched | 0.215 J/cm | 0.403 ft-lb/in | ASTM D256 |
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |