Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8330 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256A |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | reverse notched; ASTM D256 |
Ineos Nova Zylar® 221 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarityEnhanced mold releaseGood elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilization Applications: DisplaysMedical devicesOffice acc.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 3900 General Purpose Crystal Polystyrene
(discontinued **) High flow, Good compoundingApplications: Color concentrates, Compounding, Thin wall moldingsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and o.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Innovene 1088 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4C5T-013 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Antistat, and controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by F.. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature 23.0 °C |
0.375 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Flint Hills P4C6B-134A Polypropylene Homopolymer Features: Excellent processability, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Cutlery, Consumer Products, Cosmetic.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4C6Z-059 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Res.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D882 |
Spartech Polycast UF3 Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -30.0 °C |
0.375 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Izod Impact, Notched | 0.200 J/cm @Thickness 3.20 mm |
0.375 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SC 202LV General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products .. |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature -30.0 °C |
0.375 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Izod Impact, Notched | 0.200 J/cm @Temperature >=23.0 °C |
0.375 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 3590 General Purpose Crystal Polystyrene
(discontinued **) Excellent blending resin, Suitable for difficult to fill and thin wall molding, Low residuals, USP Class VIApplications: Blending applications, Single service drinkware, Medical moldingExposure to g.. |
|||
Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ISO 180 |
Ineos Nova 212 Crystal Polystyrene Low Flow Grade
(discontinued **) Excellent balance of properties; Extrusion and Injection MoldingApplications: Foam insulation, XPS food packaging, Sheet and profile extrusion, CD and DVD jewel boxesProperties were determined on i.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7635 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR .. |
|||
Izod Impact, Notched | 0.200 J/cm @Diameter 3.17 mm |
0.375 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ISO 180 |
Ineos Nova 205 Crystal Polystyrene General Purpose Grade
(discontinued **) Easy flow, Good mechanical property balance, Extrusion and Injection MoldingApplications: Sheet and film extrusion, Gloss capping, Blending with HIPS or SBSProperties were determined on injection m.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Izod Impact, Notched | 0.200 - 6.41 J/cm | 0.375 - 12.0 ft-lb/in | Average value: 0.959 J/cm Grade Count:58 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |