Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.196133 - 0.85424 J/cm @Temperature -30.0 - -18.0 °C |
0.367438 - 1.6003 ft-lb/in @Temperature -22.0 - -0.400 °F |
Average value: 0.562 J/cm Grade Count:9 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.196133 - 0.85424 J/cm @Thickness 3.17 - 6.50 mm |
0.367438 - 1.6003 ft-lb/in @Thickness 0.125 - 0.256 in |
Average value: 0.562 J/cm Grade Count:9 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.196133 - 1.07 J/cm @Temperature -30.0 - -30.0 °C |
0.367438 - 2.00 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.377 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.196133 - 1.07 J/cm @Thickness 3.17 - 6.40 mm |
0.367438 - 2.00 ft-lb/in @Thickness 0.125 - 0.252 in |
Average value: 0.377 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.196133 - 0.220 J/cm @Temperature -30.0 - -10.0 °C |
0.367438 - 0.412 ft-lb/in @Temperature -22.0 - 14.0 °F |
Average value: 0.495 J/cm Grade Count:10 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.196133 - 0.220 J/cm @Thickness 3.20 - 6.40 mm |
0.367438 - 0.412 ft-lb/in @Thickness 0.126 - 0.252 in |
Average value: 0.495 J/cm Grade Count:10 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |