Mechanical Properties Metric English Comments
Izod Impact, Notched 0.155 - 0.481 J/cm
0.290 - 0.900 ft-lb/in
Average value: 0.286 J/cm Grade Count:4
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
ASTM D256
Plenco 2308 Phenolic, Granular, Injection Molded
PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai..
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
ASTM D256
Plenco 4349 Phenolic, Granular, Transfer Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive
TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation con..
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive
TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system..
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
ASTM D256
Plenco 4311 Phenolic, Granular, Injection Molded
PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized..