Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.150 J/cm @Temperature -30.0 °C |
0.281 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycolac® INP222 ABS Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers. |
|||
Izod Impact, Notched | 0.150 - 0.200 J/cm | 0.281 - 0.375 ft-lb/in | ASTM D256 |
Prodways PLASTCure Rigid 10 500 3D Printing Polymer Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tu.. |
|||
Izod Impact, Notched | 0.150 J/cm | 0.281 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Izod Impact, Notched | 0.150 - 2.19 J/cm | 0.281 - 4.10 ft-lb/in | Average value: 0.904 J/cm Grade Count:146 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Izod Impact, Notched | 0.150 - 9.61 J/cm | 0.281 - 18.0 ft-lb/in | Average value: 1.16 J/cm Grade Count:343 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.150 J/cm | 0.281 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler
(discontinued **) Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe.. |
|||
Izod Impact, Notched | 0.150 J/cm @Temperature 23.0 °C |
0.281 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HI-2302 High Impact PBT, 30% Glass Fiber Reinforced LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 243 Toughened Polystyrene CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 246 Toughened Polystyrene Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 253 Toughened Polystyrene Characteristics High rigidity Improved toughness Good clarityProcessing Injection moldingApplications Ball pens Small appliances housings Small impellersMaterial Status: Commercial : ActiveAgenc.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 265 Toughened Polystyrene CharacteristicsGood clarity High dart impact strength High heat resistance Good stiffnessProcessing Extrusion Vacuum forming Applications Disposable glasses & bowls Deep draw formed products Ther.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 266 Toughened Polystyrene CharacteristicsGood stiffness Excellent toughness High flow Excellent clarity Processing Injection moldingApplications Transparent hangers Stationery items like pen barrels, geometric instruments .. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SPEXP 44 Antistatic Polystyrene Characteristics Easy flow Good transparency Very good flexibility Processing Extrusion Applications Transparent profiles for electrostatic dissipative packaging of small electronic components such.. |
|||
Izod Impact, Notched | 0.150 J/cm @Temperature 23.0 °C |
0.281 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.150 - 0.250 J/cm | 0.281 - 0.468 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Izod Impact, Notched | 0.150 - 0.250 J/cm | 0.281 - 0.468 ft-lb/in | ASTM D256 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Izod Impact, Notched | 0.150 - 0.250 J/cm | 0.281 - 0.468 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl.. |
|||
Izod Impact, Notched | 0.150 - 0.550 J/cm @Temperature -20.0 - 0.000 °C |
0.281 - 1.03 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 0.329 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |
|||
Izod Impact, Notched | 0.150 J/cm @Thickness 3.20 mm |
0.281 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP EXP 31 Toughened Polystyrene Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form.. |
|||
Izod Impact, Notched | 0.150 - 0.250 J/cm | 0.281 - 0.468 ft-lb/in | ASTM D256 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |
|||
Izod Impact, Notched | 0.150 - 0.686465 J/cm @Temperature -30.0 - 0.000 °C |
0.281 - 1.28603 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.283 J/cm Grade Count:14 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.150 - 10.0 J/cm @Temperature -40.0 - 0.000 °C |
0.281 - 18.7 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.495 J/cm Grade Count:13 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |