Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.26 - 8.33 J/cm | 13.6 - 15.6 ft-lb/in | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Izod Impact, Notched | 7.26 - 8.33 J/cm | 13.6 - 15.6 ft-lb/in | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Izod Impact, Notched | 0.502 - 8.33 J/cm | 0.940 - 15.6 ft-lb/in | Average value: 3.63 J/cm Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |