Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.641 - 5340 J/cm | 1.20 - 10000 ft-lb/in | Average value: 1.01 J/cm Grade Count:11 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched | 0.849 - 5340 J/cm | 1.59 - 10000 ft-lb/in | Average value: 3.88 J/cm Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Izod Impact, Notched | 0.250 - 5340 J/cm | 0.468 - 10000 ft-lb/in | Average value: 3.49 J/cm Grade Count:74 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 4.00 - 5340 J/cm | 7.50 - 10000 ft-lb/in | Average value: 13.0 J/cm Grade Count:29 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Izod Impact, Notched | 100 - 5340 J/cm | 187 - 10000 ft-lb/in | Grade Count:4 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.400 - 5340 J/cm | 0.749 - 10000 ft-lb/in | Average value: 3.00 J/cm Grade Count:60 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 0.481 - 5340 J/cm | 0.900 - 10000 ft-lb/in | Average value: 5.07 J/cm Grade Count:165 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Notched | 3.74 - 5340 J/cm | 7.00 - 10000 ft-lb/in | Average value: 4.50 J/cm Grade Count:9 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.196 - 5340 J/cm | 0.367 - 10000 ft-lb/in | Average value: 0.790 J/cm Grade Count:135 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.374 - 5340 J/cm | 0.700 - 10000 ft-lb/in | Average value: 1.46 J/cm Grade Count:180 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched | 0.427 - 5340 J/cm | 0.800 - 10000 ft-lb/in | Average value: 4.92 J/cm Grade Count:65 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Izod Impact, Notched | 0.110 - 5340 J/cm | 0.206 - 10000 ft-lb/in | Average value: 0.756 J/cm Grade Count:109 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.200 - 5340 J/cm | 0.375 - 10000 ft-lb/in | Average value: 1.44 J/cm Grade Count:54 |
Overview of materials for Polypropylene, Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.196 - 5340 J/cm | 0.367 - 10000 ft-lb/in | Average value: 0.436 J/cm Grade Count:107 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |