Polymer Property : Izod Impact, Notched = 5.00 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.200 - 5.00 J/cm
0.375 - 9.37 ft-lb/in
Average value: 0.889 J/cm Grade Count:22
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched 5.00 - 5.00 J/cm

@Temperature 0.000 - 0.000 °C
9.37 - 9.37 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 3.86 J/cm Grade Count:2
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched 4.43 - 5.00 J/cm
8.30 - 9.37 ft-lb/in
Average value: 4.81 J/cm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m..