Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 4.90 J/cm | 0.375 - 9.18 ft-lb/in | Average value: 1.64 J/cm Grade Count:9 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.430 - 4.90 J/cm | 0.806 - 9.19 ft-lb/in | Average value: 2.11 J/cm Grade Count:36 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 1.10 - 4.90 J/cm @Temperature -40.0 - -40.0 °C |
2.06 - 9.18 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 2.67 J/cm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Notched | 1.10 - 4.90 J/cm @Thickness 0.800 - 3.17 mm |
2.06 - 9.18 ft-lb/in @Thickness 0.0315 - 0.125 in |
Average value: 2.67 J/cm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |