Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.05 - 4.64493 J/cm @Temperature -40.0 - 149 °C |
1.97 - 8.70186 ft-lb/in @Temperature -40.0 - 300 °F |
Average value: 2.82 J/cm Grade Count:4 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |