Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.14 - 37.0 J/cm | 4.00 - 69.3 ft-lb/in | Average value: 10.9 J/cm Grade Count:23 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |