Mechanical Properties Metric English Comments
Izod Impact, Notched 0.37373 - 1.81526 J/cm

@Temperature -40.0 - -40.0 °C
0.70015 - 3.40073 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.08 J/cm Grade Count:4
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Izod Impact, Notched 0.260 - 1.81526 J/cm

@Temperature -50.0 - -17.8 °C
0.487 - 3.40073 ft-lb/in

@Temperature -58.0 - 0.000 °F
Average value: 0.562 J/cm Grade Count:19
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.69407 - 1.81526 J/cm

@Temperature -40.0 - 0.000 °C
1.3003 - 3.40073 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.11 J/cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Izod Impact, Notched 0.69407 - 1.81526 J/cm

@Thickness 3.17 - 3.20 mm
1.3003 - 3.40073 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 1.11 J/cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..