Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 - 0.747 J/cm | 1.00 - 1.40 ft-lb/in | Average value: 0.651 J/cm Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.534 - 0.747 J/cm | 1.00 - 1.40 ft-lb/in | Average value: 0.614 J/cm Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Izod Impact, Notched | 0.481 - 0.747 J/cm | 0.900 - 1.40 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
Izod Impact, Notched | 0.374 - 0.747 J/cm | 0.700 - 1.40 ft-lb/in | Average value: 0.587 J/cm Grade Count:10 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |