Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.0801 - 0.534 J/cm | 0.150 - 1.00 ft-lb/in | Average value: 0.191 J/cm Grade Count:51 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.340 - 0.534 J/cm | 0.637 - 1.00 ft-lb/in | Average value: 0.469 J/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.157 - 0.534 J/cm | 0.294 - 1.00 ft-lb/in | Average value: 0.280 J/cm Grade Count:13 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm @Temperature 22.8 °C |
0.800 - 1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger TECAST™ Cast Nylon (PA) TECAST™ Cast Nylon reduces downtime in heavy equipment applications. It is a low cost alternative for many non-ferrous machined parts. It has self-lubricating qualities which provide for excellen.. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm @Temperature 22.8 °C |
0.800 - 1.00 ft-lb/in @Temperature 73.0 °F |
|
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6) TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n.. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm | 0.800 - 1.00 ft-lb/in | ASTM D256 |
Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm | 0.800 - 1.00 ft-lb/in | ASTM D256 |
Aaron Industries AAROLENE® ARPS GP 100-1 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Izod Impact, Notched | 0.267 - 0.534 J/cm | 0.500 - 1.00 ft-lb/in | Average value: 0.450 J/cm Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.200 - 0.534 J/cm | 0.375 - 1.00 ft-lb/in | Average value: 0.276 J/cm Grade Count:7 |
Overview of materials for Polymethylpentene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm | 0.800 - 1.00 ft-lb/in | Average value: 0.494 J/cm Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.427 - 0.534 J/cm | 0.800 - 1.00 ft-lb/in | Average value: 0.498 J/cm Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |