Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet FullCure720 Transparent Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256A |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, Enhanced flow, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical applications.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.468 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.275 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256A |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm | 0.468 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.375 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.267 J/cm Grade Count:2 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H07D-00 Polypropylene Homopolymer Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.. |