Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.190 - 0.271 J/cm | 0.356 - 0.508 ft-lb/in | Average value: 0.224 J/cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |