Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.88 J/cm | 18.5 ft-lb/in | NB; ASTM D256 |
LyondellBasell SEQUEL® E3000 TPO Description: SEQUEL® E3000 thermoplastic olefinic elastomer (TPO) is designed for thermoformed exterior and interior applications that require toughness and dimensional stability. This extrusion.. |
|||
Izod Impact, Notched | 9.88 J/cm | 18.5 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 9.88 J/cm | 18.5 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Izod Impact, Notched | 9.88 J/cm | 18.5 ft-lb/in | Lengthwise; ASTM D256 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |