Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Izod Impact, Notched | 9.60 - 9.60 J/cm | 18.0 - 18.0 ft-lb/in | Average value: 9.60 J/cm Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound
(discontinued **) High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound
(discontinued **) High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel.. |
|||
Izod Impact, Notched | 9.60 J/cm @Temperature 23.0 °C |
18.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302V-6 LD Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 LD HC18010009 Polycarbonate is an opalescent white extrusion-grade resin containing a proprietary light diffusion package that offers an excellent combination of light.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.20 mm |
18.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Makrolon® 3258 Polycarbonate, General Purpose, Mold Release, Biocompatibility It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 6615 HS Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Adell BD-10 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Adell BD-30 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |