Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.52 J/cm | 17.8 ft-lb/in | ASTM D256 |
Ovation Polymers Opnyl OP66UT119 Nylon 66 Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All.. |