Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
17.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
17.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 2024 HS UV 425C Grey Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade
(discontinued **) Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially sui.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256; ISO 180/4A |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBRE™ 2060-6 Polycarbonate Resin Overview: CALIBRE™ 2060-6 polycarbonate resin is used in medical applications involving steam or ethylene oxide sterilization – through suitability for use in these applications is depende.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ISO 180/4A |
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Izod Impact, Notched | 9.10 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 303V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 303V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 303V-6 contains a mold release agent, a UV .. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2605 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release, Makrolon grade 2658 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2607 Polycarbonate, Injection Grade Easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially a.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2658 Polycarbonate, Injection Grade Easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer M.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2805 Polycarbonate, Injection Grade Medium flowing injection molding grade with easy mold release, Makrolon grade 2858 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separ.. |
|||
Izod Impact, Notched | 9.10 J/cm @Thickness 3.20 mm |
17.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2858 Polycarbonate, Injection Grade Medium flowing BgVV- and FDA injection molding grade, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Izod Impact, Notched | 9.10 J/cm | 17.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 827LD Nylon 6 A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer |