Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized |
|||
Izod Impact, Notched | 8.59 J/cm | 16.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 8.59 J/cm @Temperature -20.0 °C |
16.1 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East) 11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only |