Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4802-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 123SRM PC (Asia Pacific) Easy flow, uv stabilised, impact modified, super release grade polycarbonate. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Super mold release. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC35CV Polycarbonate Description: Naxel™ PC35CV is a 12 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 143 PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | natural, tints; ASTM D256 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 945U PC Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 955 PC (Asia Pacific) Lexan* 955 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in various opaque color.. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm |
15.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(6) 6 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Global PC-1418-IM Cold Temperature & Impact Modified Polycarbonate Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
KYDEX® XD 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses Features:Tough and durableResistant to cracking and chippingSolid, integral color3500+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualit.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
Kostat ICP-STAT ICS-1000 PC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp DX99854 PC LNP LUBRICOMP* DX99854 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP.. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R522 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 1102 PBT+PC Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids. |
|||
Izod Impact, Notched | 8.01 J/cm @Temperature 23.0 °C |
15.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC (Asia Pacific) Impact modified, highly chemical resistant polyester/polycarbonate alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC731 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 506 Polycarbonate Information provided by A. Schulman. |
|||
Izod Impact, Notched | 8.01 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
15.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 8.01 J/cm | 15.0 ft-lb/in | ASTM D256 |
PlastxWorld CEVIAN® A1500 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |