Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 151R PC Lexan 151R resin is a high viscosicty, nonhalogenated resin designed to be a candidate for applications produced via extrusion or blow molding processing.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 193 PC Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 22.8 °C |
14.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate Information provided by Ravago. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hylex® P1017L Polycarbonate, Unreinforced, High Flow, Mold Release Information provided by Ravago. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD121R PC Transparent/translucent PC for light diffusion special effects. MFR of 18.2. Color package may affect performance. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE121R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). MFR 18.2. Internal mold release. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-06R 6.0 MFI Grade Polycarbonate, With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® OQ4620R PC Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. |
|||
Izod Impact, Notched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® RL7517 PC FDA compliant (color limited). 2.5 MFR. Potable water/extrusion blowmolding applications.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-CL(22) 22 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B2025I Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
M. Holland Company PC522R Polycarbonate High flowHigh impact resistanceGood mold releaseApplications: AppliancesFood containersTable products |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Global PC-FR2-U-CL-902 UL Recognized 94V-2 PC Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 7.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
0.25 mm notch; ASTM D256 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene Features:Halogenated Forms:PelletsInformation provided by Multibase |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC703 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength.. |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Applied Composites 8041 Polyester SMC Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: UL 94-VO, Radiant Panel |
|||
Izod Impact, Notched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AEPC 5000-1 Engineered Polycarbonate Resin Melt flow index may be specified. |
|||
Izod Impact, Notched | 7.47 - 10.1 J/cm | 14.0 - 19.0 ft-lb/in | |
Bulk Molding Compounds BMC 695 Vinyl Ester Molding Compound BMC 695 vinyl ester molding compound is a mineral filled glass fiber-reinforced vinyl ester compound suitable for compression and injection molding It is characterized by good moldability, oil and s.. |