Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.05 J/cm | 13.2 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-0414 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 7.05 J/cm | 13.2 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-0616 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 7.05 J/cm | 13.2 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-061601 Description: Impact Modified PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 7.05 J/cm @Thickness 3.17 mm |
13.2 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-0616 Black Impact Modified Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |