Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific) LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to .. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® IR2040 PC (Europe-Africa-Middle East) IR2040 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. Food contact approved.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific) Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® VR2020 PC (Europe-Africa-Middle East) VR2020 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | >= 7.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | >= 7.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 13.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® FG1901 + PET blend (20/80) Blending KRATON FG polymers with PBT significantly improves the toughness. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second .. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl.. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC1800 PC PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Izod Impact, Notched | 7.00 J/cm @Temperature 23.0 °C |
13.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1803R PC (Asia Pacific) PC1803R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
Styrolution Luran® S KR 2864 C UV Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Izod Impact, Notched | 7.00 - 8.60 J/cm | 13.1 - 16.1 ft-lb/in | Izod tape gap; ASTM D256 |
Chengdu Polyster KLX-G11 PC Film & Sheet PC film and sheet, high transparency, both sides are polished, both sides with transparent protective films. Is printable, flame-retardant, anti-static, resists ultraviolet decay, scratch resistant,.. |
|||
Izod Impact, Notched | 7.00 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |