Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East) 40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only |
|||
Izod Impact, Notched | 6.99 J/cm | 13.1 ft-lb/in | |
Reliance Industries PBT - 35% Glass filled Information provided by Reliance Industries |
|||
Izod Impact, Notched | 6.99 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Flame Retardant, Wear Resistant. |
|||
Izod Impact, Notched | 6.99 J/cm | 13.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer 40 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched | 6.99 J/cm @Temperature 0.000 °C |
13.1 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific) 40 MFR LEXAN High Flow Ductile Copolymer |