Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.94 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM1210 PC Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 6.40 mm |
13.0 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2 PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® H2001R 23 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Designed for outdoor telecommunications enclosure applications. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
|
Samyang Trirex® PC-3020U 22 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU) RADEL® R is a Polyphenysulfone produced by Solvay Advanced Polymers. RADEL® R is in the same performance category as products like Polysulfone and ULTEM® (PEI). RADEL® R has increased performa.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Entec Hylex® P1317L1 HB Polycarbonate UV Stabilized, Higher Flow, Mold Release, Water ClearInformation provided by Entec. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers DIAMALOY 627 PC/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.94 - 8.01 J/cm | 13.0 - 15.0 ft-lb/in | |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Izod Impact, Notched | 6.94 - 9.61 J/cm | 13.0 - 18.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |