Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.87 J/cm @Temperature -20.0 °C |
12.9 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |