Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched | 6.74 J/cm | 12.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |