Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B6720 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(V20) 20 MFI UV Stabilized Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hybrid S470H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hybrid S555 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
|
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-1425 Polycarbonate, Injection Grade High FlowAdd "R" for Added ReleaseAdd "U" for UVÂ StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
12.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant UV Stable/Weatherable, f1 RatedMelt Flow Adjustable for Application UL File Number: E213588Information provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D-256 |
Glastic SG-200 Industrial Lift Magnet Glastic Grade SG-200 high-strength and high-temperature laminates offer temperature ratings of up to 210°C. SG-200 is ideal for a wide variety of product applications requiring high-temperature .. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PC FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection Molding Appearance: Clear/TransparentInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite DKE 400 PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PC/ABS 8001A Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ IM 401 18 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength an.. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N300HSL (COND, 50% RH) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 6.41 J/cm @Thickness 3.17 mm |
12.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Total MS 201 B N HDPE blow molding FINATHENE® MS 201 B N is a high density polyethylene produced by a low pressure slurry polymerization process. FINATHENE® MS 201 B N has been developed for the blow molding of Plastic Fuel Tanks a.. |
|||
Izod Impact, Notched | 6.41 J/cm @Temperature 22.8 °C |
12.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 6.41 J/cm | 12.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P1053R Polycarbonate A high flow transparent polycarbonate with good impact properties containing UV stabilizer.Data provided by the manufacturer |