Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.88 J/cm | 9.14 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant. |
|||
Izod Impact, Notched | 4.88 J/cm @Temperature 23.0 °C |
9.14 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE) LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region. |