Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D-256 |
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256-56 |
Rotuba 880 Ethyl Cellulose Data provided by the manufacturer. |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp DBS 2006 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Ultra High Impact Resistance Uses: Piping Forms: Powder Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256 |
ExxonMobil LL 5252.09 Compounding Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Izod Impact, Notched | 4.43 J/cm | 8.30 ft-lb/in | ASTM D256 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Izod Impact, Notched | 4.43 - 5.00 J/cm | 8.30 - 9.37 ft-lb/in | Average value: 4.81 J/cm Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |