Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.93 J/cm | 7.36 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America SI 9041A Silicone Compound SI 9041A is a long fiberglass reinforced silicone molding compound, which exhibits excellent high temperature properties in addition to good molding characteristics for transfer and compression mold.. |
|||
Izod Impact, Notched | 3.93 J/cm @Thickness 3.17 mm |
7.36 ft-lb/in @Thickness 0.125 in |
|
Chi Mei Polylac® PA-747S ABS - Extrusion High Impact Extrusion |