Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.45 J/cm | 6.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4019 PC Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Izod Impact, Notched | 3.45 J/cm | 6.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Izod Impact, Notched | 3.45 J/cm | 6.46 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 8250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 3.45 J/cm | 6.46 ft-lb/in | ASTM-D256 |
Braskem GM8250T HDPE High Density Extrusion Polyethylene GM8250T is a high-density polyethylene specially developed for the manufacturing of corrugated pipes. It has high molar mass and shows excellent tenacity, high stiffness, good impact resistance, and.. |