Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched | 3.25 J/cm @Temperature 0.000 °C |
6.09 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm | 6.09 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1908E Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1908E is a 20% talc filled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 3.25 J/cm @Thickness 3.20 mm |
6.09 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 8001 High Gloss, ESCR High Impact Polystyrene Characteristics Very high toughness Excellent ESCR properties against common food chemicals High gloss & heat resistance Processing Extrusion & Forming Applications Fatty food containers Co-extru.. |