Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne OnForce™ LFT NN-30 LGF/000 Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ S212 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin Good balance of physical and molding properties-high toughness, Excellent processability on high-speed, multiple-head blow molding lines, UL-94HB listedApplications: Household chemical bottles, Indu.. |
|||
Izod Impact, Notched | 2.70 J/cm @Temperature -30.0 °C |
5.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 2.70 J/cm @Temperature -30.0 °C |
5.06 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | Injection Molded; ASTM D256 |
PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 2.70 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.06 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ DP-9156-5-8000 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | |
Shell Carilon® D26CX100 Polyketone, Advanced Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26CX100 is an extrusion grade with mechanical properties that classify it as an engineering thermo.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA)
(Unverified Data**) Ixef 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss. - B.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4275 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4275 is a wear-resistant grade of polyamide-imide (PAI). This grade offers an excellent balance of mechanical properties and wear resistance. It offers high tensile strength and modulus with .. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 9245 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 2.70 J/cm @Thickness 3.17 mm |
5.06 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 710 ABS |
|||
Izod Impact, Notched | 2.70 J/cm @Thickness 3.17 mm |
5.06 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Hannam Chemical Hanalac 770 ABS, Extrusion Grade FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256A |
LyondellBasell Higlass BJ22GC Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, UV-stabilized, chemically coupled, glass fiber-reinforced polypropylene copolymer, moderately high rigidity, high impact strength, excellen.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America EM 7302XLD Long Glass Fiber Reinforced Epoxy EM 7302XLD is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirable.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030JLX1 Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Izod Impact, Notched | 2.70 J/cm @Temperature 23.0 °C |
5.06 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A35B01 Nylon 66, Chemically Coupled 35% Long Fiber A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Izod Impact, Notched | 2.70 J/cm | 5.06 ft-lb/in | ASTM D256 |
Engineered Plastics EPABS 54 ABS Injection Grade Pellets. GMP # 002. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 2.70 J/cm @Temperature 23.0 °C |
5.06 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A35N01 Nylon 66, Chemically Coupled 35% Long Fiber A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |